Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 86.2 MPa | 12500 psi | Ultimate; TM R050-38 |
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
Oxford Polymers PC 20 Unfilled Polycarbonate for Injection Molding Unfilled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
Oxford Polymers PC 46 Unfilled Polycarbonate for Blow and Extrusion Molding Unfilled Polycarbonate for Blow and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
Oxford Polymers PC 68 Unfilled Polycarbonate for Injection and Extrusion Molding Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
Oxford Polymers PC 912 Unfilled Polycarbonate for Injection and Extrusion Molding Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | 10% Def.; ASTM D695 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Compressive Strength | 86.2 MPa | 12500 psi | Break; TM R050-38 |
Resinlab® SEC1244 Silver Filled Epoxy Adhesive Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth.. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 86.0 MPa | 12500 psi | ASTM D695 |
Unitika LM-8503-10 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
Westlake Plastics Zelux® M Machine Grade Polycarbonate Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
Westlake Plastics Zelux® W Window Grade Polycarbonate Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Compressive Strength | 86.0 MPa | 12500 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Compressive Strength | 86.0 MPa @Time 360000 sec |
12500 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
3M Scotchkote™ RS 820 Epoxy Screed Scotchkote Epoxy Sceed RS 820 has been specially developed as a three component 100% solids resurfacing screed for application to concrete floor surfacesProduct Features:Combines good application ch.. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | ASTM D695 |
3M Scotchkote™ 474 Epoxy Concrete Repair Scotchkote Epoxy Concrete Repair 474 has been specifically developed as a three component 100% solids high performance mortar for use as a heavy duty repair system for concrete surfaces.Product Feat.. |
|||
Compressive Strength | 86.0 MPa | 12500 psi | ASTM D695 |
Unitika U-8000 U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | Ultimate; TM R050-38 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Strength | 86.2 MPa | 12500 psi | |
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas.. |