Polymer Property : Compressive Strength = 175000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1210 MPa
175000 psi
0°; SACMA SRM 1R-94
Zyvex Performance Materials Arovex™ 180 Carbon Nanotube Strengthened Prepreg
Arovex® 180 Prepreg is a 180°F (82°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Arovex 180 resin contains an optimum level of carbon nanotub..