Polymer Property : Compressive Strength = 19000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 131 MPa

@Temperature 23.9 °C
19000 psi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, C2 Carbonized Rayon Reinforced
Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm..
Compressive Strength 131 MPa
19000 psi
10% Def.; ASTM D695
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet)
Compressive Strength 131 MPa
19000 psi
ASTM D695
PolyOne Edgetek® PS-30GF/000 FR V0 Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedFlame RetardantPolyOne First ChoiceInformation provided by PolyOne Corporation.
Compressive Strength 131 MPa
19000 psi
ASTM D695
IDI Composites 44-10 MW Thermoset Polyester, Molding
Moderate strength material specifically formulated for microwave oven performance.Data provided by the manufacturer.
Compressive Strength 131 MPa
19000 psi
ASTM D695
IDI Composites W-102 Thermoset Polyester, Molding
Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer.
Compressive Strength 131 MPa
19000 psi
ASTM D695
Greene Tweed Arlon® 1000 Polyketone
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
Compressive Strength 131 MPa
19000 psi
Haysite 270FRII Polyester BMC, Glass Reinforced
Haysite Grade 270FRII is a second generation glass reinforced thermoset polyester bulk molding compound. This material can be compression, transfer, or injection molded. Qualified under MIL-M-14, Ty..
Compressive Strength 131 MPa

@Temperature 149 °C
19000 psi

@Temperature 300 °F
Haysite Heatmeiser® H340 Platen Insulation
Haysite’s family of mold and platen insulation products are specially engineered fiberglass reinforced thermoset polyester composites which offer superior energy efficiency, temperature control..
Compressive Strength 131 MPa
19000 psi
ASTM D695
Techmer ES Plaslube® J-4/35/TF/15 NAT PA6/12
Compressive Strength >= 131 MPa
>= 19000 psi
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter..
Compressive Strength 131 MPa
19000 psi
ASTM D695
Plenco 1581 Polyester, Pellet, Injection Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..
Compressive Strength 131 MPa

@Time 36.0 sec
19000 psi

@Time 0.0100 hour
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
Compressive Strength 131 MPa

@Temperature 23.0 °C
19000 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Compressive Strength 131 - 138 MPa
19000 - 20000 psi
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength
BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat..
Compressive Strength 131 - 165 MPa
19000 - 24000 psi
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa..
Compressive Strength 131 - 145 MPa
19000 - 21000 psi
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound
BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a..
Compressive Strength 131 - 159 MPa
19000 - 23000 psi
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie..
Compressive Strength 131 MPa
19000 psi
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro..
Compressive Strength 131 - 159 MPa
19000 - 23000 psi
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Compressive Strength 131 - 152 MPa
19000 - 22000 psi
Bulk Molding Compounds BMC 810 General Purpose Molding Compound
BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel..
Compressive Strength 131 - 145 MPa
19000 - 21000 psi
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound
BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar..
Compressive Strength 131 MPa
19000 psi
ASTM D695
Plenco 1506 Polyester, Briquette, Injection Molded
PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop..
Compressive Strength 131 MPa
19000 psi
ASTM D695
Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group
Compressive Strength 131 MPa
19000 psi
Break; TM R050-38
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
Compressive Strength 131 - 159 MPa
19000 - 23000 psi
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound
BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma..