Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 147 MPa | 21300 psi | ASTM D695 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Compressive Strength | 147 MPa | 21300 psi | ASTM D695 |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Compressive Strength | 147 MPa | 21300 psi | break; DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Compressive Strength | 147 MPa | 21300 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Compressive Strength | <= 147 MPa | <= 21300 psi | Cold Crushing Strength |
Chosun Refractories HRD-SNE Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 147 MPa | 21300 psi | Cold Crushing Strength |
Chosun Refractories SBSN-G15 Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 147 MPa | <= 21300 psi | Cold Crushing Strength |
Chosun Refractories ZNS Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 147 MPa | <= 21300 psi | Cold Crushing Strength |
Chosun Refractories CSN-601N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |