Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 237 MPa | 34400 psi | ASTM D695 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |