Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 172 MPa | 24900 psi | |
Poco Graphite SCF-2 Ion Implant Grade Graphite An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Pyrotek TS-550 Insulating Board TS-550 is phenolic-based, fiber and mineral reinforced, high-temperature material. TS-550 offers the high strength and wear resistant properties of laminated materials, while also offering the form.. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures... |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
IDI Composites M-104 Thermoset Polyester, Molding Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
IDI Composites W-103 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Sumitomo Bakelite North America FM 21386 Synthetic Fiber Reinforced Phenolic Novolac FM 21386 is a single stage phenolic molding compound reinforced with synthetic fiber in pellet form.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Plenco 6990 Phenolic, Briquette, Compression Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Plenco 4300 Phenolic, Granular, Transfer Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and .. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | Conditioned; ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Conditioned
(discontinued **) Availability: Asia Pacific; Europe; North AmericaInformation provide by Solvay Specialty Polymers |