Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 286 MPa | 41500 psi | ASTM D695 |
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant,.. |
|||
Compressive Strength | 286 MPa @Thickness 12.7 mm |
41500 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |