Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 570 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 570 MPa
82700 psi
Longitudinal
Goodfellow Carbon/Epoxy Composite Sheet
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.
Compressive Strength 570 MPa
82700 psi
Transverse
Goodfellow Carbon/Epoxy Composite Sheet
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.
Compressive Strength 570 MPa

@Treatment Temp. 20.0 °C,
Time 3600 sec
82700 psi

@Treatment Temp. 68.0 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Compressive Strength 570 MPa

@Temperature 23.0 °C
82700 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 4011 Polyimide, Yellow (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Copyright © lookpolymers.com All Rights Reserved