Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 7000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 48.3 MPa
7000 psi
10% Def.; ASTM D695
Quadrant EPP Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet)
Chemical resistance parallels PTFE Continuous use temperatures to 500°F (260°C) Compared to PTFE higher load carrying capability 1/9 of the deformation under load lower coefficient of thermal exp..
Compressive Strength 48.3 MPa
7000 psi
ASTM D695
ScanTube ECTFE Tubing
Information provided by ScanTube, Inc.
Compressive Strength 48.3 MPa
7000 psi
ASTM D695
ScanTube ETFE Tubing
Information provided by ScanTube, Inc.
Compressive Strength 48.3 MPa
7000 psi
ASTM-C773
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..
Compressive Strength 48.3 MPa
7000 psi
Cotronics Resbond™ 903HP High Temperature Ceramic Adhesive, Hi-Bond Strength
Compressive Strength 48.3 - 207 MPa
7000 - 30000 psi
Du-Co Ceramics S-470 Aluminum Silicate
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Compressive Strength 48.3 - 207 MPa
7000 - 30000 psi
Du-Co Ceramics S-699 Alumina
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Compressive Strength 48.3 MPa
7000 psi
Aremco Ceramacast™ 645-N High Temperature Potting & Casting Material Silica
Castable ceramic with low thermal conductivity.
Compressive Strength 48.3 - 55.2 MPa
7000 - 8000 psi
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Compressive Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..
Compressive Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia..
Compressive Strength 48.26 - 62.05 MPa
7000 - 9000 psi
after 816°C
Pyrotek Pyrocast ZS Refractory Shapes
Aggregate Base: Fused SilicaApplicationsTransfer troughs Information provided by Pyrotek.
Compressive Strength 48.3 MPa
7000 psi
Break; TM R050-38
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin
Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula..
Copyright © lookpolymers.com All Rights Reserved