Polymer Property : Compressive Strength = 82.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 82.0 MPa
11900 psi
ASTM D695
Unitika AXF-1500-05 Dry
Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd.
Compressive Strength 82.0 MPa
11900 psi
ASTM D695
Plenco 7487 Phenolic, Granular, Transfer Molded
PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple..
Compressive Strength 82.0 MPa
11900 psi
Absolute Drying; ASTM-D695
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Compressive Strength >= 82.0 MPa
>= 11900 psi
Ambient
China-Yixing Longly Refractories Push Slab Semi-Corundum-Mullite
Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine..