Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 57.9 MPa | 8400 psi | ASTM D695 |
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey Information provided by ITW Devcon |
|||
Compressive Strength | 57.9 MPa | 8400 psi | ASTM D695 |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |