Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 95.0 MPa | 13800 psi | Type B, 5mm/min; ISO 604:2002 |
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled) This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E.. |
|||
Compressive Strength | 95.0 MPa | 13800 psi | Type B, 5mm/min; ISO 604:2002 |
Nylacast PA6C Cast Nylon 6 Natural PA6 is the base to the other grades of material offered by Nylacast. It is available in Natural (off white) or Black colour. It is made by ionic polymerisation of e-caprolactam under anhydri.. |
|||
Compressive Strength | 95.0 MPa | 13800 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Compressive Strength | 95.0 MPa | 13800 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Compressive Strength | 95.0 MPa | 13800 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Compressive Strength | 95.0 MPa | 13800 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PA 6C WFN Cast Polyamide 6 + Wax Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Compressive Strength | 95.0 MPa | 13800 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 95.0 MPa | 13800 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 95.0 MPa | 13800 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 95.0 MPa @Strain 3.50 % |
13800 psi @Strain 3.50 % |
DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Compressive Strength | 95.0 MPa @Time 360000 sec |
13800 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Compressive Strength | 95.0 MPa | 13800 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |
|||
Compressive Strength | >= 95.0 MPa | >= 13800 psi | Ambient |
China-Yixing Longly Refractories Plate Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Compressive Strength | >= 95.0 MPa | >= 13800 psi | Ambient |
China-Yixing Longly Refractories Seggar Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |