Mechanical Properties | Metric | English | Comments |
---|---|---|---|
PENT | >= 500 hour | >= 500 hour | ASTM F 1473 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
PENT | >= 500 hour | >= 500 hour | Notch Tensile; ASTM F1473 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
PENT | >= 500 hour | >= 500 hour | ASTM F 1473 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
PENT | >= 500 hour | >= 500 hour | Notched Tensile; ASTM F1473 |
Ineos TUB 172 HDPE TUB 172 is a yellow medium density polyethylene copolymer designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stress life and slow crack growth resistance. T.. |
|||
PENT | >= 500 hour | >= 500 hour | ASTM F1473 |
Chevron Phillips Marlex® H525 High Density Polyethylene, Pressure Pipe Grade This high performance PE 4710 HDPE is tailored for demanding pressure pipe applications that require:Good long-term hoop strengthGood resistance to slow crack growthExcellent resistance to slumpAddi.. |