Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00503 GPa | 0.730 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-685A Solid Polyurethane Elastomer MDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00503 GPa | 0.730 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00503 GPa | 0.730 ksi | ASTM D-638 |
Axiall 8757 Moldings & Extrusions Flexible PVC Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00503 GPa | 0.730 ksi | ASTM D-638 |
Axiall 10705 Wire & Cable Flexible PVC Non-lead stabilized general purpose 75C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf.. |
|||
100% Modulus | 0.00503 GPa | 0.730 ksi | ASTM D-638 |
Axiall 10706 Wire & Cable Flexible PVC Non-lead stabilized 80C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall C.. |
|||
100% Modulus | 0.00503 GPa | 0.730 ksi | ASTM D-638 |
Axiall 10702 Wire & Cable Flexible PVC General purpose 80°C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |