Polymer Property : 100% Modulus = 0.995 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00686 GPa
0.995 ksi
JIS K6301
Stellarchem GP-945 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
100% Modulus 0.00686 GPa
0.995 ksi
JIS K6301
Stellarchem GP-950 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
100% Modulus 0.00686 GPa
0.995 ksi
JIS K6301
Stellarchem MP-850 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
100% Modulus 0.00686 GPa
0.995 ksi
JIS K6301
Stellarchem MP-855WR TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Copyright © lookpolymers.com All Rights Reserved