Tensile Impact Strength 105 kJ/m²
50.0 ft-lb/in²
Notched, -30°C; ISO 8256
Total 49080 UV HDPE blow molding
FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the productio..
Tensile Impact Strength 105 kJ/m²
50.0 ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Dow DMDB-7950 NT 7 High Density Polyethylene Resin
DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo..
Tensile Impact Strength 105 kJ/m²
50.0 ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Tensile Impact Strength 105 kJ/m²
50.0 ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Tensile Impact Strength 105 kJ/m²
50.0 ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1149 NT 7 is produced using UNIPOL™ PE process technology and is intended for high-speed injection molding applications. Information provided by Dow