Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7144 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as large industrial containers and trash cans. Information provide.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8320 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow GRSN-9820 NT 7 Linear Low Density Polyethylene Granular Solid DOW GRSN-9820 NT 7 is produced using UNIPOL™ PE process technology and is supplied in granular form. This resin is specifically designed as a carrier resin for color concentrates and other master .. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE) Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | ASTM D-1822 |
Axiall 7450 Rigid PVC, Extrusion Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | ASTM D-1822 |
Axiall 9211 Rigid PVC, Molding Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products.Information provided by Georgia GulfG.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | ASTM D-1822 |
Axiall 7055 Rigid PVC, Extrusion Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | ASTM D-1822 |
Axiall 7407 Rigid PVC, Extrusion Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | ASTM D-1822 |
Axiall 9153 Rigid PVC, Molding Georgia Gulf 9153 is an excellent combination of chemical resistance, impact and processing for chemically active products, such as pine oil cleaners.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Tensile Impact Strength | 168 kJ/m² | 80.0 ft-lb/in² | ASTM D-1822 |
Axiall 7055 Rigid PVC, Extrusion, White Georgia Gulf 7055 White is a special purpose rigid PVC extrusion compound designed for window and door applications. The compound exhibits the following characteristics: WeatherabilityChemical Res.. |