Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific) Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 193 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 194 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
NOVA Chemicals Novapol® HB-W555-A HDPE Blow Molding Resin Molded Plaque Properties. Features: High molecular weight, rigidity, excellent ESCR, excellent impact strength.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
NOVA Chemicals Novapol® HB-W555-AC PE Blow Molding Resin High molecular weight, High rigidity, Excellent impact strength, Excellent ESCR, Used in high purity chemical packagingInformation provided by NOVA Chemicals. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D 1822 |
NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin HB-W555-EC complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolo.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or .. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
(Unverified Data**) Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)
(discontinued **) Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
(Unverified Data**) Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)
(discontinued **) Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)
(discontinued **) Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used .. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU) Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU) Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
ExxonMobil HDPE BU46-055 High Density Polyethylene Resin Product Description: BU46-055 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Tensile Impact Strength | 420 kJ/m² | 200 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ BA46-055 Blow Molding Resin Product Description: BA46-055 is a high molecular weight high density polyethylene copolymer. It possesses a combination of excellent processability, outstanding melt strength, high impact strength.. |