Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 124R PC UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 131 PC Nonhalogenated. 3.5 MFR. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 221 PC 17.5 MFR, for small, intricate parts. Improved flame retardance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 221 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 221R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 134 PC (Asia Pacific) 3.5 MFR. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not be used for medical applicati.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 143 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 143R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Tensile Impact Strength | 546 - 580 kJ/m² | 260 - 276 ft-lb/in² | Average value: 572 kJ/m² Grade Count:4 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |