Mechanical Properties Metric English Comments
Tensile Impact Strength 399 kJ/m²

@Thickness 3.18 mm
190 ft-lb/in²

@Thickness 0.125 in
ASTM D1822
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU)
Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins...
Tensile Impact Strength 399 kJ/m²
190 ft-lb/in²
ASTM D1822
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
Tensile Impact Strength 399 kJ/m²

@Thickness 3.18 mm
190 ft-lb/in²

@Thickness 0.125 in
ASTM D1822
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU)
Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po..
Tensile Impact Strength 399 kJ/m²

@Thickness 3.18 mm
190 ft-lb/in²

@Thickness 0.125 in
ASTM D1822
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
Tensile Impact Strength 399 kJ/m²

@Thickness 3.18 mm
190 ft-lb/in²

@Thickness 0.125 in
ASTM D1822
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona..
Tensile Impact Strength 399 kJ/m²
190 ft-lb/in²
ASTM D1822
Westlake Plastics Radel® R 5500 Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c..
Tensile Impact Strength 399 kJ/m²
190 ft-lb/in²
ASTM D1822
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications
Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,..
Tensile Impact Strength 399 kJ/m²
190 ft-lb/in²
ASTM D1822
ExxonMobil HDPE HYA021L High Density Polyethylene Resin
Product Description: HYA021L is a molecular weight, high-density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: Latin A..
Tensile Impact Strength 399 kJ/m²

@Temperature -40.0 °C
190 ft-lb/in²

@Temperature -40.0 °F
ASTM D1822
ExxonMobil Paxon™ BA53-035 Blow Molding Resin  (discontinued **)
BA53-035 is a high molecular weight, high density polyethylene copolymer offering an outstanding combination of stiffness and toughness. The resin provides superior melt strength and impact resista..