Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 105 kJ/m² | 50.0 ft-lb/in² | Notched, -30°C; ISO 8256 |
Total 49080 UV HDPE blow molding FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the productio.. |
|||
Tensile Impact Strength | 105 kJ/m² | 50.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Tensile Impact Strength | 105 kJ/m² | 50.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Tensile Impact Strength | 105 kJ/m² | 50.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Tensile Impact Strength | 105 kJ/m² | 50.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1149 NT 7 is produced using UNIPOL™ PE process technology and is intended for high-speed injection molding applications. Information provided by Dow |