Polymer Property : Tensile Creep Modulus, 1 hour = 160000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 1100 - 2300 MPa
160000 - 334000 psi
Average value: 1580 MPa Grade Count:9
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Tensile Creep Modulus, 1 hour 1100 MPa
160000 psi
ISO 899-1
Lanxess Durethan® AC 30 000000 Nylon 66
PA 66, injection molding-grade, non-reinforced, higher notched impact strength than A 30 / A 31 in the dry and conditioned stateApplication Examples: plug connectors, cable binders, cable clips, par..
Tensile Creep Modulus, 1 hour 1100 MPa
160000 psi
ISO 899
BASF Ultramid® A27 E 01 PA66 (Conditioned)
Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "..
Tensile Creep Modulus, 1 hour 1100 MPa
160000 psi
ISO 899
BASF Ultramid® A34 01 PA66 (Conditioned)
Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or ..