Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Lanxess Pocan® B 1505 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 2405 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 2407 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 2605 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release, Makrolon grade 2658 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 2858 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 3108 Polycarbonate, Extrusion Grade Injection molding and extrusion grade with high viscosity, BgVV- and FDA grade for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 3208 Polycarbonate Injection molding and extrusion grade with high viscosity, BgVV- and FDA grade for food contact applications, yields especially tough parts, better resistance to hot water.Information provided by Ba.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 6485 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was .. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
Covestro Makrolon® LQ 2647 Polycarbonate, UV-Stabilized UV-stabilized injection molding grade with easy mold release, suitable for spectacle glasses (LQ = Lens Quality).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
BASF Polystyrol® 445 E WU Impact Grade Polystyrene (Europe) Easy flowing, heat-resistant, medium-impact, flame-retardant grade. Application example: electrical distribution boxes.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |
|||
Tensile Creep Modulus, 1 hour | 2200 - 2500 MPa | 319000 - 363000 psi | Average value: 2370 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Lanxess Pocan® B 1600 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |