Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.115 GPa | 16.7 ksi | ISO 1184-1983E |
LyondellBasell DP 8220M Polybutene Key Features: semi-crystalline, medium ethylene content random copolymer, reduces seal initiation temperature, FDA acceptableApplications: seal-peel layer of BOPP filmMeets FDA requirements in 21 CF.. |
|||
Modulus of Elasticity | 0.115 GPa | 16.7 ksi | |
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Modulus of Elasticity | 0.115 GPa | 16.7 ksi | |
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |