Polymer Property : Modulus of Elasticity = 0.193 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.193 GPa
28.0 ksi
ISO 1184-1983E
LyondellBasell Montell 8640 Polybutene-1
Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements..
Modulus of Elasticity 0.193 GPa
28.0 ksi
Molded Sample 2% Secant Modulus
Dow LDPE 510I Low Density Polyethylene
DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It..