Polymer Property : Modulus of Elasticity = 0.220 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.220 GPa
31.9 ksi
ISO 178
Premix Thermoplastics PRE-ELEC® PE 1270  (discontinued **)
PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 12..
Modulus of Elasticity 0.220 GPa
31.9 ksi
Secant; ASTM D638
Huntsman PE 1402 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Modulus of Elasticity 0.220 - 11.05 GPa

@Temperature -100 - 250 °C
31.9 - 1603 ksi

@Temperature -148 - 482 °F
Average value: 5.50 GPa Grade Count:19
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Modulus of Elasticity 0.220 - 11.5 GPa

@Temperature 60.0 - 150 °C
31.9 - 1670 ksi

@Temperature 140 - 302 °F
Average value: 5.24 GPa Grade Count:14
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Modulus of Elasticity 0.220 GPa
31.9 ksi
ISO 1184-1983E
LyondellBasell Montell 8340 Polybutene-1
Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements..
Copyright © lookpolymers.com All Rights Reserved