Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.740 GPa | 107 ksi | Tangent; ASTM D790 |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |