Modulus of Elasticity 115 GPa
16700 ksi
In Tension
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..
Modulus of Elasticity 115 GPa
16700 ksi
In Tension
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..
Modulus of Elasticity 115 GPa
16700 ksi
Schott N-LAK8 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Annealed
Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET.
Modulus of Elasticity 115 GPa
16700 ksi
(Annealed)
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged
Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET.
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + Annealed
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. ..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 20% Elongated Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 20% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Elongated Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + Annealed
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. ..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STOA (885°C/1hr/AC + 705°C/1hr/AC) condition. Other data below are typical of TIMETAL..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical
This entry has typical property data. Other database entries for TIMETAL® 6-2-4-6 have tensile and fatigue data for specific sample conditions.High-Strength, Intermediate Temperature AlloyFeatures..
Modulus of Elasticity 115 GPa
16700 ksi
2D
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy
Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm..
Modulus of Elasticity 115 GPa
16700 ksi
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Beta Forged + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the Beta Forged + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4..