Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 189.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip
General Elgiloy® information: High strength, ductility, fatigue life, and good mechanical properties. Corrosion resistant in numerous environments. Available in strip (currently 0.0015" to 0.075"..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, Heat Treated
Heat Treatment 5 hours at 482°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Wire, Heat Treated
Heat Treatment 5 hours at 527°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc..
Modulus of Elasticity 189.6 GPa
27500 ksi
Elgiloy® Co-Cr-Ni Alloy, Wire
The strength and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fatigue life, and..