Mechanical Properties Metric English Comments
Modulus of Elasticity 13.8 - 36.2 GPa
2000 - 5250 ksi
Average value: 27.5 GPa Grade Count:15
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Modulus of Elasticity 13.8 GPa
2000 ksi
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy
Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation.
Modulus of Elasticity 13.8 GPa
2000 ksi
Effective Modulus
Hardwire 12x-4-12 Low Density Composite
The 12X Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 12X wire cord is used where the traits of high tensile strain, excellent conformabi..
Modulus of Elasticity 13.8 GPa
2000 ksi
in <110> direction
Mateck Potassium Bromide (KBr)
Optical crystals
Modulus of Elasticity 13.8 GPa
2000 ksi
SGL Carbon Group EK 200 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Modulus of Elasticity 13.8 GPa
2000 ksi
SGL Carbon Group EK 201 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Modulus of Elasticity 13.8 GPa
2000 ksi
SGL Carbon Group V 1626 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Modulus of Elasticity 13.8 GPa
2000 ksi
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Copyright © lookpolymers.com All Rights Reserved