Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 22.1 GPa | 3200 ksi | |
SGL Carbon Group EK 20 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 22.1 GPa | 3200 ksi | |
SGL Carbon Group EK 2230 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 22.1 GPa | 3200 ksi | IPC TM-650 2.4.18.3 |
Arlon 85N Polyimide Laminate and Prepreg 85N is a polyimide and laminate prepreg system for PWBs requiring resistance to high temperature, both in process and in end-use application. Bromine-free chemistry provides thermal stability for a.. |
|||
Modulus of Elasticity | 22.1 GPa | 3200 ksi | IPC TM-650 2.4.18.3 |
Arlon 33N Polyimide Laminate and Prepreg High reliability and high temperature material33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with fla.. |