Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.193 GPa | 28.0 ksi | ISO 1184-1983E |
LyondellBasell Montell 8640 Polybutene-1 Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements.. |
|||
Modulus of Elasticity | 0.193 GPa | 28.0 ksi | Molded Sample 2% Secant Modulus |
Dow LDPE 510I Low Density Polyethylene DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It.. |