Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 200 GPa @Temperature 100 °C |
29000 ksi @Temperature 212 °F |
|
Haynes 556® alloy, 0% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 100 °C |
29000 ksi @Temperature 212 °F |
|
Haynes 556® alloy, 40% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
Crucible Steel 440A Chromium Steel Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 50 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
|
AK Steel ASTM A 1018, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ASTM A 424 Type II, VIT-PLUS® DS Enameling Carbon Steel VIT-PLUS is a controlled chemistry, non-decarburized steel designed to replace certain types of ingot products. It has good strength after fire properties. It is not recommended for direct-on cove.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ZINCGRIP® Class 2, Grade 50 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
Carpenter Micro-Melt® 9 Hardened and Tempered Tool Steel Micro-Melt® 9 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with goo.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, HSLAS, FORMABLE 40K / SAE J1392 040 XLK or 040 YLK Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (FS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 50% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 50% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703) Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless s.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 427°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | |
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | in tension |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Modulus of Elasticity | 200 GPa | 29000 ksi | RT |
Outokumpu 725LN Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |