Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.34 - 11.0 GPa | 340 - 1600 ksi | Average value: 5.60 GPa Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 2.34 - 11.0 GPa | 340 - 1600 ksi | Average value: 4.89 GPa Grade Count:22 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Modulus of Elasticity | 2.34 GPa | 340 ksi | ASTM D638 |
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM) Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep.. |