Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0300 GPa | 4.35 ksi | Wet |
Kraton® NEXAR™ MD9200 Polymer Barrier Membrane NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification a.. |
|||
Modulus of Elasticity | 0.0300 - 0.0400 GPa | 4.35 - 5.80 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Modulus of Elasticity | 0.0300 - 0.0400 GPa | 4.35 - 5.80 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Modulus of Elasticity | 0.0300 GPa | 4.35 ksi | DIN EN 826 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |