Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.87 GPa | 706 ksi | Machine; ASTM D638 |
Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates DiClad 522 and DiClad 527 use a higher fiberglass/PTFE ratio to provide mechanical properties approaching conventional substrates.Extremely Low Loss TangentExcellent Dimensional StabilityProduct Per.. |