Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.500 - 21.9 GPa | 72.5 - 3180 ksi | Average value: 2.63 GPa Grade Count:95 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Modulus of Elasticity | 0.500 - 32.0 GPa @Temperature -40.0 - 230 °C |
72.5 - 4640 ksi @Temperature -40.0 - 446 °F |
Average value: 8.06 GPa Grade Count:40 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Modulus of Elasticity | 0.500 - 1.90 GPa @Temperature 60.0 - 90.0 °C |
72.5 - 276 ksi @Temperature 140 - 194 °F |
Average value: 1.78 GPa Grade Count:8 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 0.500 - 1.10 GPa @Temperature 60.0 - 90.0 °C |
72.5 - 160 ksi @Temperature 140 - 194 °F |
Average value: 0.800 GPa Grade Count:1 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Modulus of Elasticity | 0.500 - 1.65 GPa | 72.5 - 240 ksi | Average value: 1.23 GPa Grade Count:4 |
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum.. |
|||
Modulus of Elasticity | 0.500 - 0.800 GPa @Temperature 120 - 200 °C |
72.5 - 116 ksi @Temperature 248 - 392 °F |
Average value: 0.637 GPa Grade Count:2 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Modulus of Elasticity | >= 0.500 GPa | >= 72.5 ksi | ASTM D638 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Modulus of Elasticity | 0.500 GPa | 72.5 ksi | ISO 178 |
Addiplast Addilene J 380 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Modulus of Elasticity | 0.500 - 0.900 GPa @Temperature 100 - 100 °C |
72.5 - 131 ksi @Temperature 212 - 212 °F |
Average value: 0.700 GPa Grade Count:2 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Modulus of Elasticity | 0.500 - 4.90 GPa @Temperature 60.0 - 90.0 °C |
72.5 - 711 ksi @Temperature 140 - 194 °F |
Average value: 1.37 GPa Grade Count:5 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |