Mechanical Properties Metric English Comments
Fatigue Strength 25.0 MPa

@# of Cycles 100000
3630 psi

@# of Cycles 100000
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Fatigue Strength 25.0 MPa

@# of Cycles 1.00e+7
3630 psi

@# of Cycles 1.00e+7
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.