Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 22.0 J | 16.2 ft-lb | Typical (Transverse) |
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully .. |
|||
Charpy Impact | 22.0 J @Temperature -40.0 °C |
16.2 ft-lb @Temperature -40.0 °F |
|
ThyssenKrupp XAR® 550 Structural Steel This Material Specification applies to 4 to 100 mm thick plates of the wear-resistant special structural steel XAR® 550.Application: The steel may be used for wear exposed structures, e.g. excavati.. |
|||
Charpy Impact | 22.0 J @Temperature -40.0 °C |
16.2 ft-lb @Temperature -40.0 °F |
|
ThyssenKrupp XAR® SUPRA Structural Steel This Material Specification applies to 4 to 100 mm thick plates of the wear-resistant special structural steel XAR® SUPRA.Application: The steel may be used for wear exposed structures, e.g. excava.. |
|||
Charpy Impact | 22.0 J | 16.2 ft-lb | V Notch, when tempered at 1000°F |
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13) No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa.. |
|||
Charpy Impact | 22.0 J @Temperature -18.0 °C |
16.2 ft-lb @Temperature -0.400 °F |
V-notch |
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |