Polymer Property : Charpy Impact = 65.6 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 89.0 J

@Temperature -73.0 °C
65.6 ft-lb

@Temperature -99.4 °F
V-notch
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Charpy Impact 89.0 J

@Temperature 566 °C
65.6 ft-lb

@Temperature 1050 °F
V-notch
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..