Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0121 GPa | 1.75 ksi | ASTM D790 |
Dow Engage® 8200 Polyolefin Elastomer Description: Engage® 8200 and Engage® 8207 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and performs well in a wide range of general purpose thermo.. |
|||
2% Secant Modulus | 0.0121 GPa | 1.75 ksi | ASTM D790 |
Dow Engage® 8207 Polyolefin Elastomer Description: Engage® 8207 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
2% Secant Modulus | 0.0121 GPa | 1.75 ksi | ASTM D790 |
Dow Engage® 8400 Polyolefin Elastomer Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr.. |
|||
2% Secant Modulus | 0.0121 GPa | 1.75 ksi | ASTM D790 |
Dow Engage® 8407 Polyolefin Elastomer Description: Engage® 8407 polyolefin elastomer is an ethyleneoctene copolymer with a nominal loose talc coating. The talc is untreated and has a 1µm particle size. Engage® 8407 offers excellent p.. |