Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 2010 Cyanoacrylate, gap filling PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 922 Cyanoacrylate, High temperature PERMABOND® 922 is the original allyl cyanoacrylate adhesive. It is a single part, moderate viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. P.. |
|||
Adhesive Bond Strength | 19.0 MPa | 2750 psi | |
Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | FRP Glass Epoxy, Shear; ISO 4587 |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Adhesive Bond Strength | 19.0 - 21.0 MPa | 2760 - 3050 psi | Steel, Shear; ASTM D1002 |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | ISO 4587, Shear |
Permabond 801 Cyanoacrylate, High Temperature PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | ISO 4587, Shear |
Permabond 802 Cyanoacrylate, High Temperature PERMABOND® 802 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | ISO 4587, Shear |
Permabond 820 Cyanoacrylate, High Temperature PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Adhesive Bond Strength | 19.0 MPa | 2750 psi | alum/aluminum |
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any .. |
|||
Adhesive Bond Strength | 19.0 MPa | 2750 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Epoxy Plusâ„¢ 25 Grey Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 19.0 MPa | 2750 psi | Grit blasted steel |
Loctite® Super Bonder® 495 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | >= 19.0 MPa | >= 2750 psi | ASTM D4541 |
Chesterton ARC 982 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo.. |
|||
Adhesive Bond Strength | 19.0 MPa @Temperature 82.2 °C |
2750 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-1/A Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Adhesive Bond Strength | 19.0 MPa @Temperature 25.0 °C |
2750 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-31 Epoxy Adhesive Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact.. |