Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00345 GPa | 0.500 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
300% Modulus | 0.00345 GPa @Time 7200 sec |
0.500 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7095-1000 TPE Product Description: StarMediflex P 7095-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2780 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2785H Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2860M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2870M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7650-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7660-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00345 GPa | 0.500 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |