Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00731 GPa | 1.06 ksi | ASTM D412 |
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00731 GPa | 1.06 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00731 GPa | 1.06 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |