Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0186 GPa | 2.70 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | Vulcanized |
KKPC KOSYN 1502LL Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | Vulcanized |
KKPC KOSYN 1502NF Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | Vulcanized |
KKPC KOSYN 1502W Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
Taiwan PU Corporation TPUI-G95 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
Taiwan PU Corporation TPUI-T95 Transparent Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | DIN 53504 |
Lubrizol ESTANE® T5417 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | ASTM D412 |
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
300% Modulus | 0.0186 - 0.0221 GPa | 2.70 - 3.20 ksi | Secant; Conditioned 7 days at RT/50% RH; ASTM D638 |
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0186 GPa | 2.70 ksi | ASTM D412 |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |