Mechanical Properties Metric English Comments
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Huntsman IROGRAN® PS 455-215 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 193 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester
Performance Features: Manufactures of technical parts can achieve the highest levels of: Wear and tear strengthDimensional stabilityOil resistanceLow compression setDynamic load performanceElasticit..
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412-97
Saint-Gobain Norprene® A-60-F Food Process Tubing Formulation
Description: Norprene® Food Process Tubing, Formulation A-60-F: Formulated to withstand the high temperatures frequently occurring during food and beverage processing, Norprene® Food Process..
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412-98
Saint-Gobain Norprene® A-60-G Industrial Grade Tubing Formulation
Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and appl..
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412-98
Saint-Gobain Tygon® Norprene® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems
Good for use in clean-in-place and steam-in-place cleaning and sterilization systems, Norprene® Pressure Tubing has excellent alkali resistance and is compatible with numerous oxidizing agents su..
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Teknor Apex MONPRENE® MP 2790 Thermoplastic Elastomer
Information provided by Teknor Apex Company
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Lubrizol Estane® ALR E72A Thermoplastic Polyurethane
Type: Estane® ALR E72A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..