Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Toughness | 51.0 - 541 J | 37.6 - 399 ft-lb | Average value: 220 J Grade Count:8 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Toughness | 51.0 J | 37.6 ft-lb | Per square meter |
Hexcel® HexPly® 922-1 180°C Curing Epoxy Matrix HexPly® 922-1 is a structural epoxy resin for general industrial applications and aerospace applications. HexPly® 922-1 has an exceptionally good hot/wet performance and a very high glass temperat.. |