Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 36.6 J @Temperature 22.8 °C |
27.0 ft-lb @Temperature 73.0 °F |
Dynatup Instrumented Impact; ASTM D3763 |
Spartech Royalite R84 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Impact Test | 36.6 J | 27.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Impact Test | 36.6 J | 27.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |