Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.694 J/cm @Temperature -40.0 °C |
1.30 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm, Temperature -17.8 °C |
1.30 ft-lb/in @Thickness 0.125 in, Temperature 0.000 °F |
ASTM-D256 |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 6.35 mm, Temperature -40.0 °C |
1.30 ft-lb/in @Thickness 0.250 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature -20.0 °C |
1.30 ft-lb/in @Temperature -4.00 °F |
1/8" (3mm) notched bar; ASTM D256 |
Ineos L70Z-01 Polypropylene Impact Copolymer L70Z-01 is a nucleated and antistatic high flow polypropylene medium impact copolymer for injection molding applications. This product meets the requirements of the U.S. Food and Drug Administration.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.30 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8009 FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.696 J/cm @Thickness 6.35 mm |
1.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.696 J/cm @Thickness 6.35 mm |
1.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-5302GR PBT, 30% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.696 J/cm @Thickness 6.35 mm |
1.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature -40.0 °C |
1.30 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.30 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant, Halogen Free and Impact ModifiedAppearance: BlackI.. |
|||
Izod Impact, Notched | 0.696 J/cm @Thickness 6.35 mm |
1.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-5302GR PBT, 30% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Westlake Plastics Tempalux® 5000 Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature -18.0 °C |
1.30 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 6507N Impact Copolymer Polypropylene Impact Copolymer for Injection Molding Formolene® 6507N is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional stabil.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 3320B Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3320B is a high flow random copolymer with fast cycle time and easy mold release. It is designed for injection molding appli.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256A |
ExxonMobil AP03B Polypropylene Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.30 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall SP-7221 Rigid PVC, Molding Georgia Gulf SP-7221 is a high impact rigid vinyl compound designed for water distribution systems. The product is NSF listed under Standard 14.Information provided by Georgia GulfGeorgia Gulf beca.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.30 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall UV-6685 Rigid PVC, Molding Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Info.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem INSPIRE™ 222 Performance Polypropylene Polymer INSPIRE™ 222 Performance Polymer is intended for use in extrusion and thermoforming processes. It is especially suited in applications requiring excellent clarity and good stiffness.Contains a nuc.. |