Polymer Property : Izod Impact, Notched = 2.24 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.24 J/cm

@Temperature -30.0 °C
4.20 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Noble Polymers Regis™ 275107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Izod Impact, Notched 2.24 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.20 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade
Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi..
Izod Impact, Notched 2.24 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth..
Izod Impact, Notched 2.24 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6 GF40 IM2 NAT 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth..
Izod Impact, Notched 2.24 J/cm

@Temperature 23.0 °C
4.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA
Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.24 J/cm

@Thickness 3.17 mm,
Temperature 72.8 °C
4.20 ft-lb/in

@Thickness 0.125 in,
Temperature 163 °F
ASTM D256
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc..